SOLDER COAT CO.,LTD.

Lead-free solder alloy at High strength, No Silver, low cost
/ Tough alloy CP solder LLS228N

Tensile Strength improves by addition of Sb compared with the conventional Sn-Cu Alloy composition alloy.
The shearing strength by the Thermal cycle test after mount device improves more than SAC305.
Flux spitting of flux cored solder decreases substantially.

Basic specification

Products Temp.() Sn Cu Sb Ni Ge
Solidus temp. Liquidus temp.
LLS 228N 228 230 Bal. 0.6 X 0.05 |
LLS227N(Reference) 227 227 Bal. 0.6 | 0.05 0.01

Tensile Strength

Shearing test after the thermal cycle test

Elongation

flux spitting test



close